Recently, many furniture manufacturers have shown that the adhesion of the furniture is very good at that time, but what is the reason why it is not sticky through high temperature or cabinet?
Recently, many furniture manufacturers have shown that the adhesion of the furniture is very good at that time, but what is the reason why it is not sticky through high temperature or cabinet?
- The solvent of adhesive is bonded without drying.
- The thermostability of the furniture spray adhesive/glue itself poor glue.
- Do not operate according to the requirements, resulting in uneven spraying, glue.
- The air is not cleansed to fit properly.
- When the solvent of adhesives is completely dry, then stick to the adhesive.
- Choose adhesive with good heat resistance,such as BIGGER 870k not pulverization furniture spray adhesive/glue,It placed more than 60 ℃ oven 168 hours don’t tackless and 30 days of sun exposure is completely nonchalant.
- When using furniture spray adhesive/glue should operate standard, spray uniform, do not leak glue.
- The air must be emptied and then fitted.